镁碳砖
Magnesia-Carbon Bricks
 |
Corrosion resistance against basic melt or gas |
 |
Resistance to slag penetration |
Common application:
 |
working lining in slag zone for steel furnaces and refining
vessels
|
 |
lining tap holes
|
 |
BMT
10A |
BMT
10B |
BMT
10C |
BMT
14A |
BMT
14B |
BMT
14C |
BMT
18A |
BMT
18B |
BMT
18C |
|
MgO % min |
80 |
78 |
76 |
76 |
74 |
74 |
72 |
70 |
70 |
|
C % min |
10 |
10 |
10 |
14 |
14 |
14 |
18 |
18 |
18 |
|
显气孔率Apparent
porosity, ≤ % |
4 |
5 |
6 |
4 |
5 |
6 |
3 |
4 |
5 |
|
体积密度
Density, ≥ g/cm3 |
2.90 |
2.85 |
2.80 |
2.90 |
2.82 |
2.77 |
2.90 |
2.82 |
2.77 |
|
常温耐压强度,
Cold crushing strength, ≥ MPa |
40 |
35 |
30 |
40 |
35 |
25 |
40 |
35 |
25 |
|
高温耐压强度High
temperature crushing strength (1400°C x 30min), MPa |
6 |
5 |
4 |
14 |
8 |
5 |
12 |
7 |
4 |
|